ANSI\/ASME B36.10M, Tabela danych grubości B36.19m
May 12, 2025
Zostaw wiadomość
ANSI\/ASME B36.10M, Tabela danych grubości B36.19m
| Rozmiar nominalny (cale) | Sch5s | SCH10S | Sch10 | Sch20 | Sch30 | Sch40s | Std | Sch40 | Sch60 | Sch80s | Xs | Sch80 | Sch100 | Sch120 | Sch140 | Sch160 | XXS | Sch160 |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 1/8 | 10.29 | - | 1.24 | - | - | 1.73 | 1.73 | 1.73 | 2.41 | 2.41 | 2.41 | - | - | - | - | - | - | - |
| 1/4 | 13.72 | - | 1.65 | - | - | 2.24 | 2.24 | 2.24 | 3.02 | 3.02 | 3.02 | - | - | - | - | - | - | - |
| 3/8 | 17.15 | - | 1.65 | - | - | 2.31 | 2.31 | 2.31 | 3.20 | 3.20 | 3.20 | - | - | - | - | - | - | - |
| 1/2(15) | 21.34 | 1.65 | 2.11 | - | - | 2.77 | 2.77 | 2.77 | 3.73 | 3.73 | 3.73 | - | - | - | 4.78 | 7.47 | 4.78 | - |
| 3/4(20) | 26.67 | 1.65 | 2.11 | - | - | 2.87 | 2.87 | 2.87 | 3.91 | 3.91 | 3.91 | - | - | - | 5.56 | 7.82 | 5.56 | - |
| 1(25) | 33.40 | 1.65 | 2.77 | - | - | 3.38 | 3.38 | 3.38 | 4.55 | 4.55 | 4.55 | - | - | - | 6.35 | 9.09 | 6.35 | - |
| 1 1/4(32) | 42.16 | 1.65 | 2.77 | - | - | 3.56 | 3.56 | 3.56 | 4.85 | 4.85 | 4.85 | - | - | - | - | 9.70 | - | - |
| 1 1/2(40) | 48.26 | 1.65 | 2.77 | - | - | 3.68 | 3.68 | 3.68 | 5.08 | 5.08 | 5.08 | - | - | - | - | 7.14 | 15.15 | 7.14 |
| 2(50) | 60.33 | 1.65 | 2.77 | - | - | 3.91 | 3.91 | 3.91 | 5.54 | 5.54 | 5.54 | - | - | - | - | 9.14 | 11.07 | 8.74 |
| 2 1/2(65) | 73.03 | 2.11 | 3.05 | - | - | 5.16 | 5.16 | 5.16 | 7.01 | 7.01 | 7.01 | - | - | - | - | 9.53 | 14.02 | 9.53 |
| 3(80) | 88.90 | 2.11 | 3.05 | - | - | 5.74 | 5.74 | 5.74 | 7.62 | 7.62 | 7.62 | - | - | - | - | 11.13 | 15.24 | 11.13 |
| 3 1/2(90) | 101.60 | 2.11 | 3.05 | - | - | 6.02 | 6.02 | 6.02 | 8.56 | 8.56 | 8.56 | - | - | - | 11.12 | 13.49 | 17.12 | 13.49 |
| 4(100) | 114.30 | 2.11 | 3.05 | - | - | 6.02 | 6.02 | 6.02 | 8.56 | 8.56 | 8.56 | - | - | - | 11.12 | 13.49 | 17.12 | 13.49 |
| 5(125) | 141.30 | 2.77 | 3.40 | - | - | 6.55 | 6.55 | 6.55 | 9.53 | 9.53 | 9.53 | - | - | - | 12.70 | 15.88 | 19.05 | 15.88 |
| 6(150) | 168.27 | 2.77 | 3.40 | - | - | 7.11 | 7.11 | 7.11 | 10.97 | 10.97 | 10.97 | - | - | - | 14.09 | 19.27 | 18.62 | 19.27 |
| 8(200) | 219.08 | 2.77 | 3.76 | 6.35 | 7.04 | 8.18 | 8.18 | 9.18 | 13.20 | 12.70 | 12.70 | 15.09 | 19.26 | 20.62 | 23.81 | 22.23 | 23.81 | |
| 10(250) | 273.05 | 3.40 | 4.19 | 6.35 | 7.80 | 9.27 | 9.27 | 9.27 | 12.70 | 12.70 | 12.70 | 15.09 | 19.26 | 21.44 | 25.40 | 28.58 | 25.40 | |
| 12(300) | 323.85 | 3.96 | 4.67 | 6.35 | 8.38 | 9.53 | 9.53 | 10.31 | 14.27 | 12.70 | 12.70 | 17.48 | 21.44 | 25.40 | 28.58 | 33.32 | 25.40 | |
| 14(350) | 355.60 | 3.96 | 4.78 | 6.35 | 7.92 | 9.53 | 9.53 | 11.13 | 15.09 | 12.70 | 12.70 | 19.05 | 23.81 | 27.79 | 31.75 | 35.71 | 25.40 | |
| 16(400) | 406.40 | 4.19 | 4.78 | 6.35 | 7.92 | 9.53 | 9.53 | 12.70 | 16.66 | 12.70 | 12.70 | 21.44 | 28.39 | 30.96 | 35.53 | 40.49 | 25.40 | |
| 18(450) | 457.20 | 4.19 | 4.78 | 6.35 | 7.92 | 11.13 | 9.53 | 14.27 | 19.05 | 12.70 | 12.70 | 23.81 | 29.36 | 34.33 | 38.67 | 45.24 | 25.40 | |
| 20(500) | 508.00 | 4.78 | 5.54 | 6.35 | 9.53 | 12.70 | 9.53 | 15.09 | 20.62 | 12.70 | 12.70 | 26.19 | 32.54 | 38.10 | 44.45 | 50.01 | 25.40 | |
| 22(550) | 558.80 | 4.78 | 5.54 | 6.35 | 9.53 | 12.70 | 9.53 | 22.23 | 12.70 | 12.70 | 28.58 | 34.93 | 41.26 | 47.63 | 53.98 | 25.40 | - | |
| 24(600) | 609.60 | 5.54 | 6.35 | 6.35 | 9.53 | 14.27 | 9.53 | 17.48 | 24.61 | 12.70 | 12.70 | 30.96 | 38.89 | 46.02 | 52.37 | 59.54 | - | |
| 26(650) | 660.40 | - | - | 7.92 | 12.70 | - | 9.53 | - | - | 12.70 | 12.70 | - | - | - | - | - | - | - |
| 28(700) | 711.20 | - | - | 7.92 | 12.70 | - | 9.53 | - | - | 12.70 | 12.70 | - | - | - | - | - | - | - |
| 30(750) | 762.00 | - | - | 7.92 | 12.70 | - | 9.53 | - | - | 12.70 | 12.70 | - | - | - | - | - | - | - |
| 32(800) | 812.80 | 6.35 | 7.92 | 7.92 | 12.70 | - | 9.53 | 17.48 | 12.70 | 12.70 | - | - | - | - | - | - | - | - |
| 34(850) | 863.60 | - | - | 7.92 | 12.70 | - | 9.53 | 17.48 | 12.70 | 12.70 | - | - | - | - | - | - | - | - |
| 36(900) | 914.40 | - | - | 7.92 | 12.70 | - | 9.53 | 19.05 | 12.70 | 12.70 | - | - | - | - | - | - | - | - |
| 40(1000) | 1016.00 | - | - | 9.53 | 14.3 | - | 9.53 | 26.20 | - | - | - | - | - | - | - | - | - | - |
Jaka jest różnica między nominalnymi i calowymi rurami ze stali nierdzewnej?
Rozmiar nominalny (DN):
Zazwyczaj wyrażany w milimetrach (mm) rozmiar nominalny odnosi się do przybliżonej średnicy lub wewnętrznej średnicy rury.
Jest to wartość nominalna, a nie faktyczny rozmiar rury. Na przykład,DN50Wskazuje, że średnica nominalna wynosi około 50 mm, ale faktyczna średnica zewnętrzna może być60,3 mm, w zależności od grubości ściany.
Rozmiary nominalne są szeroko stosowane w międzynarodowych standardach, szczególnie w Europie i Azji.
Rozmiar cala (NP):
Wyrażony w calach (cal) rozmiar cala odnosi się do nominalnego rozmiaru rury (NP).
Ta konwencja nazewnictwa jest powszechnie stosowana w krajach systemu cesarskiego, takich jak Stany Zjednoczone.
Na przykład,NPS 1Rura ma rzeczywistą zewnętrzną średnicę33,4 mm, nie 1 cal (25,4 mm).