EN 1.4713: Ferritic Steel Specs & Applications

Apr 07, 2026

Zostaw wiadomość

1.4713 stainless steel, commonly known as X10CrAlSi13 or UNS S13300, is a ferritic heat-resistant stainless steel with excellent oxidation resistance at elevated temperatures due to its chromium and aluminum content. The addition of aluminum promotes the formation of a highly stable, adherent aluminum oxide scale that provides superior protection against scaling and oxidation in high-temperature environments. This makes it an ideal material for applications requiring good high-temperature performance without the need for high nickel content, such as furnace components, heat treatment equipment, and automotive exhaust systems.

 

Equivalent specifications for 1.4713 stainless steel

1.4713
X10CrAlSi13, UNS S13300
Chromium-aluminum steel

 

Chemical composition of 1.4713 stainless steel

C P S
<= 0.12 0.70 - 1.40 <= 1.0 <= 0.04 <= 0.03 12.0 - 14.0 0.70 - 1.20

 

Properties of 1.4713 Stainless Steel

Yield Strength (Rp0.2)
>= 250 MPa 450 - 600 MPa >= 20% <= 200
Typical Value (800℃) ~ 30 MPa ~ 40 MPa ~ 40% -

 

Key Characteristics and Applications of 1.4713 / X10CrAlSi13

Excellent High-Temperature Oxidation Resistance: The aluminum content (0.70-1.20%) promotes the formation of a stable aluminum oxide scale that provides superior resistance to scaling and oxidation up to approximately 900℃ (1650℃F).

The ferritic structure provides good resistance to thermal cycling, making it suitable for applications with repeated heating and cooling.

Absence of nickel and low alloy content makes it significantly more economical than austenitic heat-resistant grades.

Strongly magnetic and can be welded with proper procedures, though preheating may be required.

 

Heating elements, furnace linings, burner parts, and support grids.

Retorts, muffles, and baskets for heat treating operations.

Catalytic converter supports, exhaust manifolds, and heat shields.

Burner components in gas stoves, heater parts, and fireplace inserts.

Radiant tubes and heating element sheaths.

Components in moderate-temperature process equipment.

 

How does 1.4713 compare to 1.4762 (446) and 1.4742 (X10CrAlSi18)?

1.4713 has lower chromium content (12-14%) compared to 1.4762 (446) which has 23-27% Cr, and 1.4742 (X10CrAlSi18) which has 17-19% Cr. This results in lower maximum service temperature: 1.4713 is suitable up to ~900℃, while 1.4762 can be used up to ~1100℃. The aluminum content provides additional oxidation resistance across all three grades. 1.4713 is more economical due to lower chromium content and is often chosen for applications with moderate temperature requirements (up to 900℃). For higher temperature applications (above 900℃), 1.4762 or 1.4742 with higher chromium content are recommended.

 

What are the welding considerations for 1.4713?

Welding 1.4713 requires care due to its ferritic structure and aluminum content. Key considerations include:
Low heat input welding techniques are essential to minimize grain growth in the heat-affected zone
Preheating (200-300℃) is recommended for thicker sections
Austenitic filler metals (309L, 310L) are recommended for better weld ductility
Post-weld annealing at 750-800℃ may be required to restore ductility for critical applications

 

What temperature range is 1.4713 suitable for?

1.4713 is suitable for continuous service up to approximately 900℃ (1650℃F) and intermittent service up to 950℃ (1740℃F). It maintains good oxidation resistance within this range, making it suitable for furnace components, heat treating equipment, and exhaust systems. For applications requiring higher temperature capability (above 900℃), grades with higher chromium content such as 1.4762 (446) or austenitic grades like 309/310 are recommended. The aluminum content provides excellent protection against scaling at elevated temperatures, but the material has limited creep strength above 800℃.

 

Looking for a Reliable Supplier of 1.4713 Stainless Steel?
GNEE Steel supplies cost-effective 1.4713 (X10CrAlSi13) stainless steel in plate, sheet, bar, and strip forms for moderate-temperature heat-resistant applications. We provide full material certification (EN 10204 3.1) and processing support including cutting, forming, and welding services. If you have any requirements, please feel free to contact us.

1.4713 stainless steel pipes

1.4713 stainless steel pipes

1.4713 stainless steel bars

1.4713 stainless steel bars

1.4713 stainless steel coils

1.4713 stainless steel coils

 

 

Wyślij zapytanie